Stress corrosion damage of a heat exchanger tube 1.4301 | X5CrNi18-10 | AISI 304 | S30400
| Numeric designation | 1.4301 | AISI 304 | S30400 |
|---|---|
| Chemical designation | X5CrNi18-10 |
| State | Stress corrosion damage of a heat exchanger tube |
| Etching | V2A-Beize @ 70 °C |
The classical standard austenites (V2A/V4A) can suffer SCC if tensile stresses are present and the choride content is sufficiently high. The intergranular cracks usually lead to complete component failure.