Back (Failure Cases)

WEA White Etching Area

Numeric designation1.6526
Chemical designation21NiCrMo2
Etching3 % Nital

These non-etchable white layers consist of tetragonal (i.e. non-tempered) martensite and are also referred to as grinding burn. These areas also occur in rolling bearings, often close to oxide inclusions. Causes for this zone can be: grinding burn, excessive surface pressure, slipping bearing seat, wire ropes rubbing against each other.